1. preparation
First of all, the guide roller is loaded according to the direction of the line. At the same time, the adhesive is adjusted in proportion and the heating system of the oven is started. When the corresponding setting temperature is reached, the transmission motor can be opened, and the coating can be produced.
2. coating
The substrate of the unwinding device must first pass the anilox roller, then coat with the glue, then dry the bath through the drying way, that is to finish the coating process.
3. compound
The compound process is realized after the EPC gas liquid rectify deviation enters the composite part and is bonded with the substrate of the second unwinding part.
4. cooling reel
After the cooling coil is completed, the whole production process of the substrate is completed, and the following problems should be paid attention to in production.
(1) adjust the flatness of the substrate by adjusting the position of the adjusting roll.
(2) adjusting the compound pressure between the compound rollers by adjusting the relative distance between the two compound rollers.